FERRITE AR CORES

|
MODEL |
G.W(g) |
MAINT |
N.W(g) |
||
|
A |
B |
||||
|
AR1.7% 2f14 |
0.16 |
1.7±0.1 |
14.0±0.5 |
0.15 |
|
|
AR2.8% 2f12 |
0.36 |
2.8±0.2 |
12.0±0.5 |
0.35 |
|
|
AR3/12 |
0.42 |
3.0±0.2 |
12.0±0.5 |
0.41 |
|
|
AR3.8% 2f16 |
0.90 |
3.8±0.2 |
16.0±0.5 |
0.87 |
|
|
AR4/18 |
1.14 |
4.0 |
0 |
18.0±0.5 |
1.1 |
|
-0.3 |
|||||
|
AR5.4% 2f21 |
2.38 |
5.4 |
0 |
21.0±0.5 |
2.3 |
|
-0.3 |
|||||
|
AR6/15 |
2.07 |
6.0 |
0.2 |
15.0±0.5 |
2.0 |
|
-0.3 |
|||||
|
AR6/20 |
2.69 |
6.0 |
0.2 |
20.0±0.5 |
2.6 |
|
-0.3 |
|||||
|
AR6/25 |
3.42 |
6.0 |
0.2 |
25.0±0.5 |
3.3 |
|
-0.3 |
|||||
|
AR6/30 |
4.15 |
6.0 |
0.2 |
30±0.5 |
4.0 |
|
-0.3 |
|||||
|
AR6/45 |
6.22 |
6.0 |
0.2 |
45±0.8 |
6.0 |
|
-0.3 |
|||||
|
AR6/70 |
9.53 |
6.0 |
0.2 |
70±7.0 |
9.2 |
|
-0.3 |
|||||
|
AR8/20 |
4.97 |
8.0±0.2 |
20.0±0.5 |
4.8 |
|
|
AR8% 2f25 |
6.22 |
8.0±0.2 |
25.0±0.5 |
6 |
|
|
AR8% 2f30 |
7.46 |
8.0±0.2 |
30.0±0.5 |
7.2 |
|
|
AR8/45 |
11.19 |
8.0±0.2 |
45.0±0.5 |
10.8 |
|
|
AR8/70 |
17.51 |
8.0±0.3 |
70.0±0.8 |
16.9 |
|
|
AR8/90 |
22.49 |
8.0±0.3 |
90.0±1.0 |
21.7 |
|
|
AR10/24 |
9.33 |
9.75±0.25 |
24.0±0.5 |
9.0 |
|
|
AR10/30 |
11.71 |
10.0±0.2 |
30.0±0.5 |
11.3 |
|
|
AR12.5% 2f100 |
60.50 |
12.5±0.2 |
100.0±1.5 |
58.5 |
|
|
AR14/45 |
34.00 |
14.0±0.3 |
45.0±0.5 |
32.81 |
|
|
AR17.5/185 |
186.00 |
17.3±0.25 |
185.0±2.0 |
180 |
|